OBRABOTKAMETALLOV MATERIAL SCIENCE Vol. 27 No. 2 2025 a b c d Fig. 6. Transmission electron microscopy images of Ti49.2Ni50.8 alloy after current-assisted rolling to ε=0.4 at various magnifications: ×6000 (a), ×8000 (b), ×30000 (c); and to ε =1.4 (d) a b Fig. 7. Transmission electron microscopy images of Ti50.0Ni50.0 alloy during current-assisted rolling: to ε = 0.8 (a); to ε = 1.4 (b)